AMS 7725E class2 Tungsten Alloy Bar

AMS 7725E class2 tungsten alloy bar has high density, high melting point (3410°C), high electrical resistance, low thermal expansion, and good thermal conductivity. It can be used as medical facility and evaporation boat.

AMS 7725E class2 tungsten alloy bar pictureThe properties of AMS 7725E class2 tungsten alloy bar are:
Matrix: 92.5% W
Density: 17.15~17.85g/cc
Hardness Rockwell Max: 33HRC
AMS 7725E: Class2 Type1
Ultimate Tensile Strength: 94 KSI and 648 MPa
Yield Strength (0.2% offset): 75 KSI and 517 MPa
Elongation: 2%
AMS 7725E: Class2 Type2
Ultimate Tensile Strength: 110 KSI and 758 MPa
Yield Strength (0.2% offset): 75 KSI and 517 MPa
Elongation: 5%